詳細說明
Thermanit DW
符合:EN 1600 AWS A 5.4 Mat. No.
E 22 12 R 3 2 E309-17 1.4829
說明:Resistant to scaling up to 950 °C (1742 °F). For joining andsurfacing applications on matching/similar heat resistant steels/cast steel grades.
對擴大到950°C(1742°F)。加入和
出現應用程序匹配/類似的耐熱鋼 鑄鋼的成績。
適用母材:TüV certified parent metalX15CrNiSi20-12 (1.4828); AISI 305; ASTM A297HF
熔敷金屬化學成分:%
C Si Mn Cr Ni
0.11 <0.9 0.8 22.5 12.5
熔敷金屬力學性能
Heat- Yield strength Yield strength Tensile Elongation Impact values
treatment 0.2% 1.0% strength (L0=5d0) in J CVN
N/mm2 N/mm2 N/mm2 %
AW 320 340 550 30 55 |
|