ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/ELECTRODAG PR-406B電子組裝/工業(yè)膠水/電子組裝膠水/工業(yè)用膠
技術(shù)服務(wù)熱線:021-51693135 / 021-22818476
Electrodag PR-406B carbon polymer thick film ink is suitablefor application on most rigid substrates.
TYPICAL PROPERTIES OF UNCURED MATERIAL
Solids Content by Weight, % 56 to 60
Viscosity Brookfield , 20 rpm @ 20°C, mPa•s (cP) 35,000 to
45,000
Density, kg/cm3 1,250
Shelf Life @ 5 to 30°C (from date of manufacture), year 1
Flash Point oC 54
TYPICAL SCREEN PRINTING PROCESS
Recommended Thickness
Applied dry coating thickness , μm 12 to 15
Emulsion Thickness
Emulsion Thickness , μm 20 to 40
Recommended Screen Type
Monofilament polyester screen , threads/cm 61 to 90
Stainless steel screen , threads/cm 77 to 110
Recommended Squeegee
Material removed from containers maybe contaminated during use. Do not return product to theoriginal container. 漢高 Corporation cannot assumeresponsibility for product which has been contaminated orstored under conditions other than those previously indicated.
Electrodag PR-406B碳聚合物厚膜油墨是合適的適用于大多數(shù)剛性基材。
固化材料的典型特性
固體含量按重量計(jì),%56至60
粘度Brookfield,20rpm,20℃,mPa•s(cP)35,000〜
45,000
密度,kg /cm31,250
保質(zhì)期5至30°C(從制造日期起),第1年
閃點(diǎn)oC54
典型屏幕印刷工藝
推薦厚度
應(yīng)用干涂層厚度,μm12〜15
乳液厚度 |