詳細說明
Thermanit GEW 316L-17
符合: EN 1600 AWS A 5.4 Mat. No.
E 19 12 3 L R 3 2 E316L-17 1.4430
說明:Stainless; resistant to intercrystalline corrosion and wetcorrosion up to 400 °C (752 °). Corrosion resistant similar to
matching low carbon and stabilized austenitic 18/8 CrNiMosteels/cast steel grades.For joining and surfacing applications with matching/similar –
non stabilized and stabilized – austenitic CrNi(N) and CrNiMo(N)steels/cast steel grades.
不銹鋼,耐晶間腐蝕和濕腐蝕400°C(752°)。耐腐蝕相似匹配低碳和穩定奧氏體CrNiMo 18/8鋼/鑄鋼的成績。加入,忽而應用程序與匹配/類似不穩定和穩定奧氏體CrNi(N)和CrNiMo(N)鋼/鑄鋼的成績。
適用母材:TüV certified parent metals
X10CrNiMoNb18-12 (1.4583) X2CrNiMoN17-13-3 (1.4429)
S31653; AISI 316L, 316Ti, 316Cb
熔敷金屬化學成分:% C Si Mn Cr Mo Ni
<0.04 <0.9 0.8 19.0 2.8 12.5
熔敷金屬力學性能
Heat- Yield strength Yield strength Tensile Elongation Impact values
treatment 0.2% 1.0% strength (L0=5d0) in J CVN
N/mm2 N/mm2 N/mm2 %
AW 350 380 580 35 60 (+20 °C)
40 (–105 °C) |
|